Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Beijing Chemical Industry KAIFA® M106 MPPO Resin

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer Beijing Chemical Industry Research Institute (Group)
Trade Name KAIFA®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Chemical Industry KAIFA® M106 MPPO Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, High thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 88.0 MPa
12800 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO179
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 3.20 mm
V-1

@Thickness 0.126 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 2.7

@Frequency 1e+6 Hz
2.7

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm

@Thickness 2.00 mm
508 kV/in

@Thickness 0.0787 in
ASTM D149
Dissipation Factor 0.0030

@Frequency 1e+6 Hz
0.0030

@Frequency 1e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Rear Barrel Temperature 260 °C
500 °F
Middle Barrel Temperature 280 °C
536 °F
Front Barrel Temperature 280 °C
536 °F
Nozzle Temperature 275 °C
527 °F
Mold Temperature 80.0 °C
176 °F
Injection Pressure 120 MPa
17400 psi
Cycle Time - Injection 35 sec
35 sec
Screw Speed 70 rpm
70 rpm