Processing Properties Metric English Comments
Pot Life 9.00 - 180 min
9.00 - 180 min
Average value: 64.2 min Grade Count:28
Overview of materials for Epoxy Adhesive, Flexible
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro..