Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.910 - 1.28 g/cc
0.0329 - 0.0462 lb/in³
Average value: 1.07 g/cc Grade Count:3
Water Absorption 0.700 - 12.2 %
0.700 - 12.2 %
Average value: 4.98 % Grade Count:14
Viscosity 550 - 350000 cP
550 - 350000 cP
Average value: 27500 cP Grade Count:27
Mechanical Properties Metric English Comments
Hardness, Shore A 21.0 - 94.0
21.0 - 94.0
Average value: 56.4 Grade Count:5
11.0 - 98.0

@Temperature 0.000 - 75.0 °C
11.0 - 98.0

@Temperature 32.0 - 167 °F
Average value: 45.6 Grade Count:6
Hardness, Shore D 60.0 - 89.0
60.0 - 89.0
Average value: 79.3 Grade Count:15
15.0 - 90.0

@Temperature -60.0 - 75.0 °C
15.0 - 90.0

@Temperature -76.0 - 167 °F
Average value: 73.8 Grade Count:14
Tensile Strength, Ultimate 0.172 - 86.6 MPa
25.0 - 12600 psi
Average value: 23.7 MPa Grade Count:20
Elongation at Break 3.20 - 190 %
3.20 - 190 %
Average value: 78.0 % Grade Count:20
Shear Strength 1.45 - 41.9 MPa
210 - 6080 psi
Average value: 19.2 MPa Grade Count:20
0.690 - 36.887 MPa

@Temperature -55.0 - 121 °C
100 - 5350.0 psi

@Temperature -67.0 - 250 °F
Average value: 12.6 MPa Grade Count:20
Adhesive Bond Strength 9.65 - 36.5 MPa
1400 - 5300 psi
Average value: 25.7 MPa Grade Count:8
1.72369 - 30.3369 MPa

@Temperature -54.4 - 82.2 °C
250.000 - 4400.01 psi

@Temperature -66.0 - 180 °F
Average value: 16.9 MPa Grade Count:8
Peel Strength 5.26 - 7.01 kN/m
30.0 - 40.0 pli
Average value: 6.57 kN/m Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 13.0 - 73.0 µm/m-°C
7.22 - 40.6 µin/in-°F
Average value: 34.8 µm/m-°C Grade Count:6
Glass Transition Temp, Tg 42.0 - 115 °C
108 - 239 °F
Average value: 73.8 °C Grade Count:6
Electrical Properties Metric English Comments
Electrical Resistivity 4.00e+8 - 4.40e+16 ohm-cm
4.00e+8 - 4.40e+16 ohm-cm
Average value: 2.22e+15 ohm-cm Grade Count:14
2.90e+7 - 2.50e+13 ohm-cm

@Temperature 100 - 150 °C
2.90e+7 - 2.50e+13 ohm-cm

@Temperature 212 - 302 °F
Average value: 1.03e+12 ohm-cm Grade Count:10
Processing Properties Metric English Comments
Processing Temperature 20.0 - 149 °C
68.0 - 300 °F
Average value: 68.7 °C Grade Count:12
Cure Time 120 - 120 min

@Temperature 80.0 - 80.0 °C
2.00 - 2.00 hour

@Temperature 176 - 176 °F
Average value: 120 min Grade Count:2
Pot Life 9.00 - 180 min
9.00 - 180 min
Average value: 64.2 min Grade Count:28