Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 8.00 - 10.0 min | 8.00 - 10.0 min | |
Northstar Polymers MPP-A50A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Pot Life | 8.00 - 10.0 min | 8.00 - 10.0 min | |
Northstar Polymers MPP-A90A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Pot Life | 8.00 min | 8.00 min | |
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer This two-component polyurethane casting system makes type of soft elastomer material known as “gel”. Applications for this material include filling component for computer keyboard/mouse-pad wrist.. |
|||
Pot Life | 8.00 - 12.0 min @Temperature 25.0 °C |
8.00 - 12.0 min @Temperature 77.0 °F |
|
Resin Technology Group TIGA 108 Room Temperature Curing Epoxy Adhesive 1 to1 mix ratio by volume.TIGA 108 is an epoxy adhesive system that provides excellent bond strength to most substrates. Recommended for production bonding applications, this low viscosity formulati.. |
|||
Pot Life | 8.00 - 10.0 min | 8.00 - 10.0 min | |
Northstar Polymers GK-7 Low Viscosity Polyurethane Gel Cast This material is formulated for production of thin polyurethane gel film or parts. The low viscosity property of the mixed component enables the user to cast this into a thin layer without entrappi.. |
|||
Pot Life | 8.00 - 11.0 min | 8.00 - 11.0 min | |
Northstar Polymers MPP-A65A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Pot Life | 8.00 - 7200 min | 8.00 - 7200 min | Average value: 670 min Grade Count:33 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Pot Life | 8.00 min @Temperature 23.9 °C |
8.00 min @Temperature 75.0 °F |
|
ITW Devcon Flexane® Rubber Repair / Castable Urethane Fast Cure Liquid, Grey Information provided by ITW Devcon |
|||
Pot Life | 8.00 min @Temperature 23.9 °C |
8.00 min @Temperature 75.0 °F |
|
ITW Devcon Flexane® Rubber Repair / Castable Urethane Fast Cure, Black Information provided by ITW Devcon |