Polymer Property : Pot Life = 12.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 8.00 - 12.0 min

@Temperature 25.0 °C
8.00 - 12.0 min

@Temperature 77.0 °F
Resin Technology Group TIGA 108 Room Temperature Curing Epoxy Adhesive
1 to1 mix ratio by volume.TIGA 108 is an epoxy adhesive system that provides excellent bond strength to most substrates. Recommended for production bonding applications, this low viscosity formulati..
Pot Life 10.0 - 12.0 min

@Temperature 25.0 °C
10.0 - 12.0 min

@Temperature 77.0 °F
Permabond ET5401 Epoxy Resin
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..
Pot Life 11.0 - 12.0 min
11.0 - 12.0 min
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel
SAI-1 is custom formulated polyurethane gel material to yield very soft elastomer gel material from low viscosity components at room temperature. This material is variable mixing ratio so that the ..
Pot Life 7.00 - 12.0 min

@Temperature 23.9 °C
7.00 - 12.0 min

@Temperature 75.0 °F
Devcon Combo Wear FC Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.