Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 8.00 - 11.0 min | 8.00 - 11.0 min | |
Northstar Polymers MPP-A65A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |