Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 40 - 50 min | 40 - 50 min | |
NextGen Adhesives P907-26 Optical Assembly Adhesive Description: NGAC P907-26 is a low viscosity and room temperature curing adhesive specifically formulated for optical applications where clarity is critical.Advantages and Applications: Uses include.. |
|||
Pot Life | 30 - 50 min | 30 - 50 min | 100 gram mass |
Master Bond EP21ARHT Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a convenient 100 to 50 mix ratio by weight an.. |
|||
Pot Life | 30 - 50 min | 30 - 50 min | 100 gram mass |
Master Bond EP21ARHTND Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a convenient 100 to 50 mix ratio by weight and is formulat.. |
|||
Pot Life | 40 - 50 min | 40 - 50 min | 100 gram batch |
Master Bond EP38CL Adhesive Features Toughness and Durability Description: Master Bond EP38CL is a lower viscosity, optically clear two component epoxy system for high performance bonding, coating, sealing and small encapsulations, featuring toughness and dura.. |
|||
Pot Life | 40 - 50 min | 40 - 50 min | 100 gram mass |
Master Bond Supreme 11AN Two Component, Heat Resistant Epoxy Adhesive Description: Master Bond Polymer Adhesive System Supreme 11AN is a two component thermally conductive heat resistant epoxy adhesive with a one-to-one mix ratio, by weight or volume. It readily devel.. |