Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 2.50 - 4320 min | 2.50 - 4320 min | Average value: 373 min Grade Count:65 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Pot Life | 2880 - 4320 min @Temperature 23.9 °C |
2880 - 4320 min @Temperature 75.0 °F |
100 gram batch |
Master Bond EP112LS Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation Master Bond EP112LS is a low viscosity two component epoxy resin system for potting, encapsulation, sealing, coating and impregnation. The mix ratio is an easy to use 100:80 by weight. EP112LS offer.. |