Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Pot Life = 2.50 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MGB-A80AQ High Performance Polyurethane Cast Elastomer System 80A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MGB-A90A High Performance Polyurethane Cast Elastomer System 90A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MSS-A85BQ High Performance Polyurethane Cast Elastomer System 85A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MSS-A85C Ester Base Polyurethane
This high performance polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhibit hig..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MSS-A90A High Performance Polyurethane Cast Elastomer System 90A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MGG-A70DQ High Performance Polyurethane Cast Elastomer System 70A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires some load-bearing, slide abrasion, constant water contac..
Pot Life 2.50 - 4320 min
2.50 - 4320 min
Average value: 373 min Grade Count:65
Overview of materials for Epoxy, Cast, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr..