Polymer Property : Pot Life = 3.00 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MGB-A80AQ High Performance Polyurethane Cast Elastomer System 80A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MGB-A90A High Performance Polyurethane Cast Elastomer System 90A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MSS-A85BQ High Performance Polyurethane Cast Elastomer System 85A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MSS-A85C Ester Base Polyurethane
This high performance polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhibit hig..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MSS-A90A High Performance Polyurethane Cast Elastomer System 90A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Pot Life 2.00 - 3.00 min

@Temperature 23.0 °C
2.00 - 3.00 min

@Temperature 73.4 °F
Permabond TA4202 Toughened Acrylic Adhesive
PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MGG-A70DQ High Performance Polyurethane Cast Elastomer System 70A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires some load-bearing, slide abrasion, constant water contac..