Processing Properties Metric English Comments
Pot Life 140 min
140 min
Dow Corning 7-9800 SOFT SKIN ADHESIVE KIT (A&B)
Two-part, platinum-catalyzed, unfilled silicone elastomeric adhesive. This a clear and soft skin adhesive for wound care dressings, transdermal drug delivery, or pharmaceutical topical applications...
Pot Life 140 min
140 min
500 g
Abatron AboCast 50-3/AboCure 50-1 Epoxy
Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.Processin..