Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 140 min | 140 min | |
Dow Corning 7-9800 SOFT SKIN ADHESIVE KIT (A&B) Two-part, platinum-catalyzed, unfilled silicone elastomeric adhesive. This a clear and soft skin adhesive for wound care dressings, transdermal drug delivery, or pharmaceutical topical applications... |
|||
Pot Life | 140 min | 140 min | 500 g |
Abatron AboCast 50-3/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.Processin.. |