Pot Life 30.0 - 100000 min
30.0 - 100000 min
Average value: 5460 min Grade Count:19
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..