Polymer Property : Hot-Working Temperature = 1150 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Hot-Working Temperature 1150 - 1180 °C
2100 - 2150 °F
Then more rapidly
Schmolz + Bickenbach 416 Stainless Steel Bar
Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity..
Hot-Working Temperature 1150 - 1180 °C
2100 - 2150 °F
Then more rapidly
Schmolz + Bickenbach 416RS Stainless Steel Bar
Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc..
Hot-Working Temperature 1150 - 1220 °C
2100 - 2230 °F
Heat in range
Schmolz + Bickenbach UGIMA® 304 Cu Stainless Steel Bar
Description: 304Cu UGIMA® is an enhanced machining grade produced only by Ugitech, providing the ultimate level of machinability available in an non-resulfurized austenitic stainless steel. 304Cu..
Hot-Working Temperature 1150 - 1220 °C
2100 - 2230 °F
Heat in range
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar
Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM..