Processing Properties Metric English Comments
Die Opening 0.0889 - 0.216 cm
0.0350 - 0.0850 in
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin
FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0..
Die Opening 0.0889 - 0.203 cm
0.0350 - 0.0800 in
Recommended range
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film
FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
Die Opening 0.0889 - 0.216 cm
0.0350 - 0.0850 in
Recommended range
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins
FPs117-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without ..
Die Opening 0.0889 - 0.216 cm
0.0350 - 0.0850 in
Recommended range
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
Die Opening 0.0889 - 0.216 cm
0.0350 - 0.0850 in
Average value: 0.151 cm Grade Count:4
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum..