Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Mineral Filled, NCG Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.14 - 1.38 g/cc
0.0412 - 0.0497 lb/in³
Average value: 1.25 g/cc Grade Count:10
Filler Content 5.00 - 25.0 %
5.00 - 25.0 %
Average value: 14.4 % Grade Count:9
Water Absorption 0.700 - 1.50 %
0.700 - 1.50 %
Average value: 1.16 % Grade Count:9
Linear Mold Shrinkage 0.00100 - 0.0150 cm/cm
0.00100 - 0.0150 in/in
Average value: 0.00430 cm/cm Grade Count:10
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 68.9 - 207 MPa
10000 - 30000 psi
Average value: 116 MPa Grade Count:10
Elongation at Break 0.500 - 5.00 %
0.500 - 5.00 %
Average value: 2.03 % Grade Count:10
Modulus of Elasticity 5.17 - 13.1 GPa
750 - 1900 ksi
Average value: 8.41 GPa Grade Count:10
Flexural Yield Strength 103 - 324 MPa
15000 - 47000 psi
Average value: 172 MPa Grade Count:10
Flexural Modulus 4.48 - 12.4 GPa
650 - 1800 ksi
Average value: 7.74 GPa Grade Count:10
Izod Impact, Notched 0.374 - 2.14 J/cm
0.700 - 4.01 ft-lb/in
Average value: 0.780 J/cm Grade Count:10
Izod Impact, Unnotched 3.20 - 5.34 J/cm
6.00 - 10.0 ft-lb/in
Average value: 3.74 J/cm Grade Count:9
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 243 - 266 °C
470 - 510 °F
Average value: 251 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 232 - 260 °C
450 - 500 °F
Average value: 243 °C Grade Count:7
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:7
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 100 ohm-cm
1.00 - 100 ohm-cm
Average value: 14.1 ohm-cm Grade Count:10
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 117000 ohm Grade Count:10
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:7
Processing Properties Metric English Comments
Processing Temperature 266 - 293 °C
510 - 560 °F
Average value: 280 °C Grade Count:9
Mold Temperature 65.6 - 107 °C
150 - 225 °F
Average value: 89.4 °C Grade Count:10
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
Average value: 94.2 MPa Grade Count:9