Processing Properties Metric English Comments
Processing Temperature 80.0 - 95.0 °C

@Time 3600 sec
176 - 203 °F

@Time 1.00 hour
Henkel Turco 4338-L Jet Engine Cleaner
Turco 4338-L is a two-part liquid, alkaline permanganate formulation developed specifically for jet engine cleaning. It modifies high temperature heat scale by chemically changing the structure of t..
Processing Temperature 23.0 - 95.0 °C
73.4 - 203 °F
Henkel Turco Rust Bloc Jet Engine Cleaner
Turco Rust Bloc is an alkaline liquid used as a rust inhibiting rinse additive or cleaner. It provides temporary in-plant rust protection for steel and cast iron.Applications:Metal Processing LinesJ..
Processing Temperature 80.0 - 95.0 °C

@Time 3600 sec
176 - 203 °F

@Time 1.00 hour
Henkel Turco T-4181L Liquid Alkaline Rust Remover
Turco T-4181L (Liquid Alkaline Rust Remover) is an amber, liquid compound formulated to remove rust, paints, lube oils, drawing pastes, cutting oils and protective oils from ferrous alloys by immers..