Polymer Property : Processing Temperature = 626 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301-7329/GY PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301-7449 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301-7648/BK PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically ..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301-7836 PPS, linear, with glass fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts.High dim..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301-7932 PPS, linear, with aramid reinforcement and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage ..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301-8066 PPS, linear, with carbon fiber, lubricant modified, high viscosity
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301-8095 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.High chemic..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 20/XCF/30 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 20/XCF/35 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 20-0791 Polyphthalamide, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 20-0916 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 20-7687 Polyphthalamide, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 20-7868 Polyphthalamide, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 20-7913 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 20-8283 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 20-8302 Polyphthalamide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 21-7976 Polyamide 6/6T, with glass fiber and PTFE, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Processing Temperature 330 °C
626 °F
mass temp
Lehmann & Voss LUVOCOM® 1301-8305 PPS, linear, with glass fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam..
Processing Temperature 330 °C
626 °F
Average value: 330 °C Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..