Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addcomp ADD-VANCE® SA 192 Slip Masterbatch, LDPE base

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Addcomp
Trade Name ADD-VANCE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp ADD-VANCE® SA 192 Slip Masterbatch, LDPE base.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fields of application: Improves slip properties of polyolefins. It can also be used as a release agent for injection molded productsExamples: (L)LDPE, HDPE, and PP films, sheets, profiles, injection molded products, etc.Mode of action and advantages: ADD-VANCE SA 192 provides excellent slip properties. ADD-VANCE SA 192 reduces friction between two surfaces for instance between polymer and metal. As a consequence the slip properties of the product are improvedAdvantages: Highly effective, fast migration slip agent, already at low dosing rates; Injection molding: also improved demoulding and product release; Non-sticking pellets, dust free; and Safe and easy handlingRegulations: ADD-VANCE SA 192 is suitable for use in a wide range of plastics that come into contact with food.Information provided by ADDCOMP
Processing Properties Metric English Comments
Processing Temperature <= 250 °C
<= 482 °F
Descriptive Properties Value Comments
Appearance Translucent granules
Dosing Level 0.01
as a mould
0.75-2%