Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 232 - 257 °C | 450 - 495 °F | Average value: 249 °C Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |