Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 401D, Nylon 6 Injection molding grade. Dry as molded. Nylene 401D is a specially formulated nylon 6 molding resin possessing outstanding flow characteristics. Nylene 401D is ideally suited for applications requi.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 404 Nylon 6 Injection molding grade. Dry as molded. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In additi.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 404 Nylon 6, 50% RH Injection molding grade. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In addition to protection.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 406 Nylon 6, 50% RH Injection molding grade. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from 406 have bet.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 406F Nylon 6, 50% RH Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling molding resin.
.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 409 Nylon 6 Dry as molded. Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 409 Nylon 6, 50% RH Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid m.. |
|||
Processing Temperature | 232 - 272 °C | 450 - 522 °F | |
Nylene® 826 Nylon Copolymer Dry as molded. Nylene 826 is a special nylon copolymer suitable for both blown and cast film co-extrusion. Nylene 826 has a lower melt point and is less crystalline than standard nylon 6 resins. In.. |
|||
Processing Temperature | 232 - 272 °C | 450 - 522 °F | |
Nylene® CX3395 Nylon Copolymer Dry as molded. Nylene CX3395 is a higher RV version of 826 which is a special nylon copolymer suitable for both blown and cast film co-extrusion. Nylene CX3395 has a lower melt point and is less cr.. |
|||
Processing Temperature | 232 - 268 °C | 450 - 514 °F | Extrusion |
Chevron Phillips Marlex® HXM 50100-02 Extra high molecular weight hexene copolymer
(discontinued **) Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesCharacteristics:.. |
|||
Processing Temperature | <= 232 °C | <= 450 °F | injection molding |
Chevron Phillips K-Resin® KR01 Styrene-Butadiene Copolymer, Injection Molding Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC can be processed by injection molding and extrusion into attractive useful parts that have excellent clarity, good toughness, good stiffness, h.. |
|||
Processing Temperature | <= 232 °C | <= 450 °F | injection molding |
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t.. |
|||
Processing Temperature | <= 232 °C | <= 450 °F | injection molding |
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give .. |
|||
Processing Temperature | 232 - 268 °C | 450 - 514 °F | Extrusion |
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Processing Temperature | 232 °C | 450 °F | Film extrusion temperature |
Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045.02AC Polyethylene resin is a high stability blown film extrusion resin that provides excellent tear strength and outstanding toughness. It contains high level of slip additive and medi.. |
|||
Processing Temperature | 232 °C | 450 °F | Film extrusion temperature |
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056 Polyethylene resin is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 .. |
|||
Processing Temperature | 232 °C | 450 °F | Film extrusion temperature |
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr.. |
|||
Processing Temperature | 232 - 270 °C | 450 - 518 °F | Average value: 250 °C Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Processing Temperature | 232 - 270 °C | 450 - 518 °F | Average value: 249 °C Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |