Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 404 Nylon 6 Injection molding grade. Dry as molded. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In additi.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 406F Nylon 6 Dry as molded. Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 409 Nylon 6, 50% RH Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid m.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 452 Nylon 6 Dry as molded. Injection molding grade. Nylene 452 is a plasticized, injection molding nylon for use in applications requiring high flexibility, and excellent toughness and abrasion resistance. Bec.. |
|||
Processing Temperature | 232 °C | 450 °F | |
Nylene® 603 Nylon 6, Extrusion Grade Dry as molded. Extrusion grade. Nylene 603 is a plasticized, high residual monomer resin designed for extrusion applications requiring excellent flexibility, high strength and good abrasion resist.. |
|||
Processing Temperature | 232 - 272 °C | 450 - 522 °F | |
Nylene® 826 Nylon Copolymer Dry as molded. Nylene 826 is a special nylon copolymer suitable for both blown and cast film co-extrusion. Nylene 826 has a lower melt point and is less crystalline than standard nylon 6 resins. In.. |
|||
Processing Temperature | <= 232 °C | <= 450 °F | |
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding. Molded parts provide excellent part detail on fast production cycles. Molded parts have excellent c.. |
|||
Processing Temperature | <= 232 °C | <= 450 °F | injection molding |
Chevron Phillips K-Resin® KR01 Styrene-Butadiene Copolymer, Injection Molding Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC can be processed by injection molding and extrusion into attractive useful parts that have excellent clarity, good toughness, good stiffness, h.. |
|||
Processing Temperature | <= 232 °C | <= 450 °F | injection molding |
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give .. |
|||
Processing Temperature | 232 °C | 450 °F | Film extrusion temperature |
Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045.02AC Polyethylene resin is a high stability blown film extrusion resin that provides excellent tear strength and outstanding toughness. It contains high level of slip additive and medi.. |
|||
Processing Temperature | 232 °C | 450 °F | Film extrusion temperature |
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and.. |
|||
Processing Temperature | 232 - 257 °C | 450 - 495 °F | Average value: 249 °C Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |