Polymer Property : Processing Temperature = 255 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 245 - 255 °C
473 - 491 °F
Barrel Temperature
SABIC PP 521P Polypropylene Homopolymer for Bi-axially Oriented Film
Product Description: PP 521P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r..
Processing Temperature 245 - 255 °C
473 - 491 °F
Barrel Temperature
SABIC PP 523P Polypropylene Homopolymer for Bi-axially Oriented Film
Product Description: PP 523P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r..
Processing Temperature 245 - 255 °C
473 - 491 °F
Barrel Temperature
SABIC PP 524P Polypropylene Homopolymer for Bi-axially Oriented Film
Product Description: PP 524P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r..
Processing Temperature 245 - 255 °C
473 - 491 °F
Barrel Temperature
SABIC PP 529P Polypropylene Homopolymer for Bi-axially Oriented Film
Product Description: PP 529P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r..
Processing Temperature 245 - 255 °C
473 - 491 °F
Wave Soldering
Nihon Superior SN96Cl Lead-Free Solder Alloy
Processing Temperature 215 - 255 °C
419 - 491 °F
Zhejiang Juner 301-G0 Flammable Resistant
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
Processing Temperature 215 - 255 °C
419 - 491 °F
Zhejiang Juner 301-G10 10% Glass Fibre Reinforced and Flammable Resistant
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
Processing Temperature 225 - 255 °C
437 - 491 °F
Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6
Applications: Mid-Grade CBInformation provided by Zhejiang Juner New Materials Co, Ltd.
Processing Temperature 235 - 255 °C
455 - 491 °F
EBM Processing Melt Temp.
Eastman Tritan WX500 Copolyester
Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generati..
Processing Temperature 235 - 255 °C
455 - 491 °F
EBM Processing Melt Temp.
Eastman Tritan WX510 Copolyester
Eastman Tritan WX510 is a transparent blue resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. ..