Processing Properties Metric English Comments
Processing Temperature 235 - 250 °C
455 - 482 °F
Barrel Temperature
SABIC PP 500P Polypropylene Homopolymer for Raffia Applications
Product Description: PP 500P is specially developed for producing stretched tapes with the following features:Consistent processabilityEasy orientationLow water carry overGood mechanical properties..
Processing Temperature 235 - 250 °C
455 - 482 °F
Barrel Temperature
SABIC PP 502P Polypropylene Homopolymer for Raffia Applications
Product Description: PP 502P is intended for producing low denier stretched tapes with the following features:Consistent processabilityGood processability at high line speedsLow water carry overGoo..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter for film or coating with EVA or EVOH
DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin  (discontinued **)
Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® 3048 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® 3095 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® 3120 Acid-/Acrylate-Modified EVA Adhesive Resin  (discontinued **)
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® E326 Acid-/Acrylate-Modified EVA Adhesive Resin  (discontinued **)
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® 3101 Acid-/Acrylate-Modified EVA Adhesive Resin
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter for film or coating with EVA or EVOH
DuPont Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter for film or coating with EVA or EVOH
DuPont Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter for film or coating with EVA or EVOH
DuPont Bynel® 4164 Anhydride-Modified LLDPE Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter for film or coating with EVA or EVOH
DuPont Bynel® 41E556 Anhydride-Modified LLDPE Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter for film or coating with EVA or EVOH
DuPont Bynel® 4206 Anhydride-Modified LDPE Adhesive Resin
Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process ..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter for film or coating with EVA or EVOH
DuPont Bynel® 4208 Anhydride-Modified LDPE Adhesive Resin
Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process ..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® E418 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Processing Temperature 235 °C
455 °F
Tipco Tipcofil® AU 027 - Unfilled Nylon-6 Compound, with High Heat Stability, for Injection Molding
Unreinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Processing Temperature 235 °C
455 °F
Suggested extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® 1124 Modified EVA Adhesive Resin
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® 3810 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® 3930 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Processing Temperature 235 - 255 °C
455 - 491 °F
EBM Processing Melt Temp.
Eastman Tritan WX510 Copolyester
Eastman Tritan WX510 is a transparent blue resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. ..
Processing Temperature <= 235 °C
<= 455 °F
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate
Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a ..
Processing Temperature <= 235 °C
<= 455 °F
DuPont™ Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Processing Temperature 235 °C
455 °F
Recommended Extrusion Temperature
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Processing Temperature 235 °C
455 °F
Recommended Extrusion Temperature
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Processing Temperature 235 °C
455 °F
Recommended Extrusion Temperature
Arkema Group Pebax® 7033 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Processing Temperature 235 °C
455 °F
Recommended Extrusion Temperature
Arkema Group Pebax® Rnew 70R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 70R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter.
DuPont Bynel® 2169 Anhydride-Modified Ethylene Acrylate Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter.
DuPont Bynel® 2174 Anhydride-Modified Ethylene Acrylate Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter. Degrades above 238°C.
DuPont Bynel® 3933 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Copyright © lookpolymers.com All Rights Reserved