Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Barrel Temperature |
SABIC PP 520L Polypropylene Homopolymer for Tubular Water Quenched Film Product Description: PP 520L is specially developed for tubular water quenched blown film applications with a suitable dosage of slip and antiblock additives.Films produced using PP 520L will exhib.. |
|||
Processing Temperature | 195 - 215 °C | 383 - 419 °F | |
Taiwan Sheen Soon Sheenthane® A9600R Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 195 - 215 °C | 383 - 419 °F | |
Taiwan Sheen Soon Sheenthane® D6050 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 215 °C | 320 - 419 °F | Extrusion |
Dyna-Purge® F Purging Compound Designed for Sheet & Profile Extrusion & Single-Layer Blown FilmGeneral Description:DYNA-PURGE F is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, with a proprie.. |
|||
Processing Temperature | 195 - 215 °C | 383 - 419 °F | |
Wanhua Chemical Wanthane® WHT-1195 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 195 - 215 °C | 383 - 419 °F | |
Wanhua Chemical Wanthane® WHT-1198 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 195 - 215 °C | 383 - 419 °F | |
Wanhua Chemical Wanthane® WHT-7190 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 195 - 215 °C | 383 - 419 °F | |
Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 195 - 215 °C | 383 - 419 °F | |
Wanhua Chemical Wanthane® WHT-2198 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 180 - 215 °C | 356 - 419 °F | |
ExxonMobil Santoprene® 8201-80HT Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material offers enhanced tensile, tear and abrasion properties along with improve.. |
|||
Processing Temperature | 170 - 215 °C | 338 - 419 °F | |
Celanese 525 Film LDPE polymer for flexible packaging and molding 525 is a high strength resin, recommended for shrink films and general purpose packaging. Properties listed are for a film produced on a 20:1 L/D, 65 mm extruder with a 130 mm die, at a stock tempe.. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 6045D Thermoplastic Polyurethane Elastomer Zythane™ 6045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistan.. |
|||
Processing Temperature | 200 - 215 °C | 392 - 419 °F | hot runner |
Celanese RITEFLEX 435 TPC, Unfilled Riteflex« 435 is a Thermoplastic Polyester Elastomer with a 35 nominal Shore D hardness, low modulus and outstanding low temperature impact strength and tear resistance.Information provided by Cela.. |
|||
Processing Temperature | 190 - 215 °C | 374 - 419 °F | hot runner |
Celanese RITEFLEX 440 TPC, Unfilled Riteflex 440 is a nominal 40 Shore D thermoplastic polyester elastomer with medium modulus.Information provided by Celanese |
|||
Processing Temperature | 195 - 215 °C | 383 - 419 °F | |
Wanhua Chemical Wanthane® WHT-1595 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 195 - 215 °C | 383 - 419 °F | |
Wanhua Chemical Wanthane® WHT-2195 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly.. |
|||
Processing Temperature | 195 - 215 °C | 383 - 419 °F | hot runner |
Celanese Hostaform® CP15X POM, Unfilled Preliminary Data SheetInformation provided by Celanese |