Polymer Property : Processing Temperature = 191 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 177 - 191 °C
350 - 375 °F
Recommended Stock Temperature
Sylvin Technologies 5748 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Processing Temperature 177 - 191 °C
350 - 375 °F
Recommended Stock Temperature
Sylvin Technologies 6046 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Processing Temperature 157 - 191 °C
315 - 375 °F
Average value: 174 °C Grade Count:46
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..