Sylvin Technologies 6046 PVC Wire/Cable Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Sylvin Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 6046 PVC Wire/Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore C 75
75
At 10 seconds
Tensile Strength, Ultimate 20.0 MPa
2900 psi
Elongation at Break 360 %
360 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air <= 105 °C
<= 221 °F
Brittleness Temperature -12.0 °C
10.4 °F
Oxygen Index 25.6 %
25.6 %
Processing Properties Metric English Comments
Processing Temperature 177 - 191 °C
350 - 375 °F
Recommended Stock Temperature