Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 157 °C | 315 °F | Optimal Thermoforming temperature for sheet 0.25-1.0 cm (0.10-0.39 in) |
Plaskolite Duraplex® SG-05 Sign Grade Acrylic Sheet, Impact Modified Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Processing Temperature | 157 - 168 °C | 315 - 335 °F | Recommended Stock Temperature |
Sylvin Technologies 5100 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 157 - 191 °C | 315 - 375 °F | Average value: 174 °C Grade Count:46 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |