Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 177 - 188 °C | 350 - 370 °F | Recommended Stock |
S&E Specialty Polymers TufFlex™ GTPE-9070J-34 TPE Compound Application: A 105°C rated, UV resistant, matte finish, TPE alloy jacketing compound for FT4 and riser applications.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 177 - 188 °C | 350 - 370 °F | Recommended Stock |
S&E Specialty Polymers TufFlex™ GTPE-98-186B PVC Compound Application: A 90°C, dull, PVC alloy jacketing compound.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 177 - 188 °C | 350 - 370 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-1030 PVC Compound Application: A 60°C, TW, THW PVC based insulation compound.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 177 - 188 °C | 350 - 370 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-1038 Natural 85 PVC Compound Application: A 60 - 75°C general purpose, sunlight resistant compound suitable for jacketing applications.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 182 - 188 °C | 360 - 370 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-1046HLF PVC Compound Application: A RoHS compliant, 105?C rated PVC compound, suitable for thin wall insulation and designed to pass VW-1 flame test requirements.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 182 - 188 °C | 360 - 370 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-1046LF PVC Compound Application: A 105°C, lead free, tri-rated semi-rigid insulation compound suitable for UL style 1061, CSA-SR-PVC, MIL-I-16878.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 182 - 188 °C | 360 - 370 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-3099LF PVC Compound Application: RoHS compliant, 80°C AWM insulation and jacketing compoundInformation provided by S&E Specialty Polymers |
|||
Processing Temperature | 171 - 188 °C | 340 - 370 °F | Recommended Stock Temperature |
Sylvin Technologies 60509 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 177 - 188 °C | 350 - 370 °F | Recommended Stock Temperature |
Sylvin Technologies 6055 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |