Polymer Property : Processing Temperature = 105 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 105 - 171 °C
221 - 340 °F
Film Forming Surface Temperature
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film
Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc..
Processing Temperature 105 - 171 °C
221 - 340 °F
Film Forming Surface Temperature
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film
Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista..
Processing Temperature 105 - 171 °C
221 - 340 °F
Film Forming Surface Temperature
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film
UV Screening, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistan..
Processing Temperature 105 - 171 °C
221 - 340 °F
Film Forming Surface Temperature
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film
Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,..