Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 105 - 171 °C | 221 - 340 °F | Film Forming Surface Temperature |
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc.. |
|||
Processing Temperature | 105 - 171 °C | 221 - 340 °F | Film Forming Surface Temperature |
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista.. |
|||
Processing Temperature | 105 - 171 °C | 221 - 340 °F | Film Forming Surface Temperature |
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film UV Screening, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistan.. |
|||
Processing Temperature | 105 - 171 °C | 221 - 340 °F | Film Forming Surface Temperature |
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,.. |