Polymer Property : Processing Temperature = 1020 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 1020 - 1050 °C
1870 - 1920 °F
Hardened then air cooled
Misumi DC53 JIS Tool Steel
General purpose cold work die and mold steel whose strength and toughness approach those of high speed steels. Good machinability and grindability. Tougher than D2 Tool Steel. Machines 30% faster th..
Processing Temperature 1020 °C
1870 °F
Flow Temp
Wieland Bio Porta 1020 Solder
Solder supplied as strip (0.18 oz. roll)Information provided by WielandDental
Processing Temperature 1020 °C
1860 °F
fusing temperature
Wall Colmonoy COLMONOY® 98 - Nickel-Based Alloy With Chromium Carbide
Description and Application: Nickel-based alloy with superior resistance to corrosive liquids. Low coefficient of friction to reduce metal-to-metal adhesive wear loss.Method of Application: Spraywe..