Polymer Property : Processing Temperature = 1860 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 1020 °C
1860 °F
fusing temperature
Wall Colmonoy COLMONOY® 98 - Nickel-Based Alloy With Chromium Carbide
Description and Application: Nickel-based alloy with superior resistance to corrosive liquids. Low coefficient of friction to reduce metal-to-metal adhesive wear loss.Method of Application: Spraywe..