Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 1020 - 1050 °C | 1870 - 1920 °F | Hardened then air cooled |
Misumi DC53 JIS Tool Steel General purpose cold work die and mold steel whose strength and toughness approach those of high speed steels. Good machinability and grindability. Tougher than D2 Tool Steel. Machines 30% faster th.. |