Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.76 J/g-°C @Temperature 288 °C |
0.660 BTU/lb-°F @Temperature 550 °F |
|
Duratherm 600 Paraffinic Heat Transfer Fluid Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to .. |
|||
Specific Heat Capacity | 2.76 J/g-°C @Temperature 260 °C |
0.660 BTU/lb-°F @Temperature 500 °F |
|
Duratherm 630 Paraffinic Heat Transfer Fluid Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F.. |
|||
Specific Heat Capacity | 2.76 J/g-°C @Temperature 260 °C |
0.660 BTU/lb-°F @Temperature 500 °F |
|
Duratherm FG Paraffinic Heat Transfer Fluid Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac.. |