Thermal Properties Metric English Comments
Specific Heat Capacity 2.76 J/g-°C

@Temperature 288 °C
0.660 BTU/lb-°F

@Temperature 550 °F
Duratherm 600 Paraffinic Heat Transfer Fluid
Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to ..
Specific Heat Capacity 2.76 J/g-°C

@Temperature 260 °C
0.660 BTU/lb-°F

@Temperature 500 °F
Duratherm 630 Paraffinic Heat Transfer Fluid
Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F..
Specific Heat Capacity 2.76 J/g-°C

@Temperature 260 °C
0.660 BTU/lb-°F

@Temperature 500 °F
Duratherm FG Paraffinic Heat Transfer Fluid
Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac..