Polymer Property : Specific Heat Capacity = 1.32 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.32 J/g-°C

@Temperature 50.0 °C
0.315 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona..
Specific Heat Capacity 1.32 J/g-°C

@Temperature 50.0 °C
0.315 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di..