Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.850 J/g-°C @Temperature 20.0 °C |
0.203 BTU/lb-°F @Temperature 68.0 °F |
|
Solvay Chemicals Perchloroethylene Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay |
|||
Specific Heat Capacity | 0.850 J/g-°C @Temperature 50.0 °C |
0.203 BTU/lb-°F @Temperature 122 °F |
|
Carlisle 201HD Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |
|||
Specific Heat Capacity | 0.850 J/g-°C @Temperature 50.0 °C |
0.203 BTU/lb-°F @Temperature 122 °F |
|
Carlisle 201LL Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |
|||
Specific Heat Capacity | 0.850 J/g-°C @Temperature 50.0 °C |
0.203 BTU/lb-°F @Temperature 122 °F |
|
Carlisle 201HL Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |
|||
Specific Heat Capacity | 0.850 J/g-°C @Temperature 50.0 °C |
0.203 BTU/lb-°F @Temperature 122 °F |
|
Carlisle 201LD Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |