Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.203 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.850 J/g-°C

@Temperature 20.0 °C
0.203 BTU/lb-°F

@Temperature 68.0 °F
Solvay Chemicals Perchloroethylene
Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay
Specific Heat Capacity 0.850 J/g-°C

@Temperature 50.0 °C
0.203 BTU/lb-°F

@Temperature 122 °F
Carlisle 201HD Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Specific Heat Capacity 0.850 J/g-°C

@Temperature 50.0 °C
0.203 BTU/lb-°F

@Temperature 122 °F
Carlisle 201LL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Specific Heat Capacity 0.850 J/g-°C

@Temperature 50.0 °C
0.203 BTU/lb-°F

@Temperature 122 °F
Carlisle 201HL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Specific Heat Capacity 0.850 J/g-°C

@Temperature 50.0 °C
0.203 BTU/lb-°F

@Temperature 122 °F
Carlisle 201LD Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Copyright © lookpolymers.com All Rights Reserved