Specific Heat Capacity 0.673 J/g-°C

@Temperature 1100 °C
0.161 BTU/lb-°F

@Temperature 2010 °F
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr
Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h..
Specific Heat Capacity 0.673 J/g-°C

@Temperature 1100 °C
0.161 BTU/lb-°F

@Temperature 2010 °F
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 2 hr
Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h..
Specific Heat Capacity 0.673 J/g-°C

@Temperature 1100 °C
0.161 BTU/lb-°F

@Temperature 2010 °F
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr
Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h..
Specific Heat Capacity 0.673 J/g-°C

@Temperature 1100 °C
0.161 BTU/lb-°F

@Temperature 2010 °F
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr
Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h..
Specific Heat Capacity 0.673 J/g-°C

@Temperature 1100 °C
0.161 BTU/lb-°F

@Temperature 2010 °F
Carpenter BioDur™ CCM® Medical Implant Alloy, Annealed
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..
Specific Heat Capacity 0.673 J/g-°C

@Temperature 1100 °C
0.161 BTU/lb-°F

@Temperature 2010 °F
Carpenter BioDur™ CCM® Medical Implant Alloy, Warm Worked
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..
Specific Heat Capacity 0.673 J/g-°C

@Temperature 1100 °C
0.161 BTU/lb-°F

@Temperature 2010 °F
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur CCM Plus alloy is a..
Specific Heat Capacity 0.673 J/g-°C

@Temperature 1100 °C
0.161 BTU/lb-°F

@Temperature 2010 °F
Carpenter BioDur™ CCM® Medical Implant Alloy, Hot Worked
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..