Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name BioDur™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur CCM Plus alloy is a wrought powder metallurgy product produced by vacuum induction melting (VIM) followed by inert gas atomization and hot isostatic pressing to produce 100% dense billets. These billets are then processed by conventional steel-making practices to make finished products.BioDur™ and CCM Plus™ are trademarks of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Density 8.28 g/cc
0.299 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 400
400
Estimated from Rockwell C for Brinell test with 3000 kg load, 10 mm ball.
Hardness, Knoop 437
437
Estimated from Rockwell C
Hardness, Rockwell C 43
43
Hardness, Vickers 418
418
Estimated from Rockwell C
Tensile Strength, Ultimate 1365 MPa
198000 psi
Tensile Strength, Yield 930 MPa

@Strain 0.200 %
135000 psi

@Strain 0.200 %
Elongation at Break 22 %
22 %
in 4D
Reduction of Area 17 %
17 %
Thermal Properties Metric English Comments
CTE, linear 12.8 µm/m-°C

@Temperature 0.000 - 100 °C
7.11 µin/in-°F

@Temperature 32.0 - 212 °F
13.1 µm/m-°C

@Temperature 25.0 - 300 °C
7.30 µin/in-°F

@Temperature 77.0 - 572 °F
14.7 µm/m-°C

@Temperature 25.0 - 700 °C
8.18 µin/in-°F

@Temperature 77.0 - 1290 °F
16.92 µm/m-°C

@Temperature 25.0 - 1000 °C
9.400 µin/in-°F

@Temperature 77.0 - 1830 °F
Specific Heat Capacity 0.452 J/g-°C

@Temperature 23.0 °C
0.108 BTU/lb-°F

@Temperature 73.4 °F
0.590 J/g-°C

@Temperature 600 °C
0.141 BTU/lb-°F

@Temperature 1110 °F
0.673 J/g-°C

@Temperature 1100 °C
0.161 BTU/lb-°F

@Temperature 2010 °F
Thermal Conductivity 12.766 W/m-K

@Temperature 23.0 °C
88.596 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
25.264 W/m-K

@Temperature 600 °C
175.33 BTU-in/hr-ft²-°F

@Temperature 1110 °F
35.022 W/m-K

@Temperature 1177 °C
243.05 BTU-in/hr-ft²-°F

@Temperature 2151 °F
Component Elements Properties Metric English Comments
Carbon, C 0.20 - 0.30 %
0.20 - 0.30 %
Chromium, Cr 26 - 30 %
26 - 30 %
Cobalt, Co 66 %
66 %
as remainder
Molybdenum, Mo 5.0 - 7.0 %
5.0 - 7.0 %
Nitrogen, N 0.15 - 0.20 %
0.15 - 0.20 %