Polymer Property : Specific Heat Capacity = 0.406 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.70 J/g-°C

@Temperature 200 °C
0.406 BTU/lb-°F

@Temperature 392 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra..
Specific Heat Capacity 1.70 J/g-°C

@Temperature 200 °C
0.406 BTU/lb-°F

@Temperature 392 °F
DSC
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Specific Heat Capacity 1.70 J/g-°C

@Temperature 200 °C
0.406 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable..
Specific Heat Capacity 1.70 J/g-°C

@Temperature 200 °C
0.406 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..