Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 67.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |