Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 67.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.