Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific)
Designed for outdoor telecommunications enclosure applications.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific)
Designed for outdoor telecommunications enclosure applications.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 364 PBT+PC
Designed for outdoor telecommunications enclosure applications.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 364 PBT+PC
Designed for outdoor telecommunications enclosure applications.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® 364 PBT
This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® 364 PBT
This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® 5220U PBT+PC
Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® 5220U PBT+PC
Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific)
Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific)
Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR
LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR
LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR (Asia Pacific)
LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR (Asia Pacific)
LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Copyright © lookpolymers.com All Rights Reserved