Polymer Property : CTE, linear, Parallel to Flow = 39.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL6414 PC
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific)
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East)
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific)
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Europe-Africa-Middle East)
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® ML7652 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Medium flow, excellent low temperature ductility.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Colorcomp D10009 PC
LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied ..
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Colorcomp D10009 PC (Asia Pacific)
LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied ..
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP FARADEX PS003E PA 6
LNP* FARADEX* PS003E is a compound based on Nylon 6 resin containing 15% Stainless Steel. Added features of this material include: EMI/RFI Shielding.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific)
LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Europe-Africa-Middle East)
LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC
LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing 10% PTFE and 10% Aramid Fiber. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific)
LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT
LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret..
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific)
LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret..
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA
LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific)
LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC
Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East)
Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly
LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific)
Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability.
CTE, linear, Parallel to Flow 70.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON ME003S PP
LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized.