Polymer Property : CTE, linear, Parallel to Flow = 30.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC
LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing 10% Glass Beads and 15% PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC
LNP* LUBRICOMP* DFL369XF is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant.
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC
LNP* LUBRICOMP* DFL369XF is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant.
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature 60.0 - 138 °C
30.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 815 PBT
15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific)
LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS
LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral.
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East)
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E..
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific)
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature 60.0 - 138 °C
30.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific)
15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp 9X04488 POLYPHENYLENESULFONE
LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific)
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC (Asia Pacific)
LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific)
LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.
CTE, linear, Parallel to Flow 54.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific)
LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.