Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature 40.0 - 120 °C
15.1 µin/in-°F

@Temperature 104 - 248 °F
ASTM E 831
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6
LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature 40.0 - 120 °C
15.1 µin/in-°F

@Temperature 104 - 248 °F
ASTM E 831
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific)
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific)
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DE006ER PC
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DE006ER PC
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific)
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific)
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.