Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 38.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific) Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications. |
|||
CTE, linear, Parallel to Flow | 38.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific) Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications. |
|||
CTE, linear, Parallel to Flow | 38.0 µm/m-°C @Temperature 100 - 150 °C |
21.1 µin/in-°F @Temperature 212 - 302 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b.. |
|||
CTE, linear, Parallel to Flow | 37.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36S PA 66 LNP* LUBRICOMP* RFL36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 37.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXY PA 66 LNP* LUBRICOMP* RFL36XXY is a compound based on Nylon 66 containing 30% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 37.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 LNP* LUBRICOMP* RFL36XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 38.0 µm/m-°C @Temperature 100 - 150 °C |
21.1 µin/in-°F @Temperature 212 - 302 °F |
4 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over.. |
|||
CTE, linear, Parallel to Flow | 38.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific) LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 38.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66 LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
CTE, linear, Parallel to Flow | 38.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific) LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 38.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66 LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 38.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Asia Pacific) PPE+PS blend. 10% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including wate.. |