Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 37.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RFL36S PA 66
LNP* LUBRICOMP* RFL36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized.
CTE, linear, Parallel to Flow 37.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXY PA 66
LNP* LUBRICOMP* RFL36XXY is a compound based on Nylon 66 containing 30% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
CTE, linear, Parallel to Flow 37.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66
LNP* LUBRICOMP* RFL36XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.